#methodological rigourSingle-flake testing leaves reproducibility insufficiently established
The principal devices are patterned on one flake, and absolute efficiency is reported for one device. The 20 consecutive acquisitions quantify short-term measurement precision rather than independent-flake or device-to-device variability.
↳ Fig. 2b,c; Fig. 4a caption; Fig. 4b,c
#methodological rigourResonance mechanism lacks quantitative experimental separation
No measured Q factor establishes its individual contribution to enhancement. The measured response near 1,650 nm also differs from the 1,550-nm design, with angular and finite-size broadening complicating quantitative comparison.
↳ Fig. 1b and inset; FTIR discussion; enhancement-mechanism discussion following Fig. 4a
#positioningEqual efficiency requires unequal pump intensities
The approximately 10^-4 efficiency is reached at 562 GW cm−2, compared with approximately 100 GW cm−2 for the cited 1.2-µm quasi-phase-matched stack. The comparison establishes a thickness advantage, not matched-intensity efficiency superiority.
↳ Absolute-efficiency comparison following Fig. 4c