#methodological rigourSurface misfit undermines the additivity conclusion
Concentration effects vary substantially across the tested materials, while lack of fit remains significant even after log transformation. The claim that factors can be adjusted independently therefore exceeds what the fitted interaction tests establish, and one material per particle-size level also confounds the quadratic interpretation.
↳ Sections 2.6, 3.1, and 4.2; Tables 2–3; Conclusion (2)
#methodological rigourProtocol and assay gaps limit interpretation
Injection-cycle counts and treatment volumes are not specified, and aggregation or variability of the three axial UCS sections is not reported. The 0.075 mm sieve used after acid washing also risks losing soil from silt with a median particle size of 0.075 mm, compromising carbonate estimates without a recovery safeguard.
↳ Sections 2.1 and 2.3–2.5
#positioningMechanistic confirmation exceeds the acknowledged evidence
The companion carbonate and microscopy observations support an association with strength, but do not establish direct attribution of the BBD strengths. Conclusion (4) nevertheless claims mechanistic confirmation despite Section 4.1 stating that targeted measurements are still needed.
↳ Sections 3.3 and 4.1; Table 7; Conclusion (4)