# Sustainable Production of Ultrathin Ge Freestanding Membranes

- **DOI:** [10.3390/su16041444](https://doi.org/10.3390/su16041444)
- **Rating:** Sound (3.1 out of 5)
- **Verdict:** Wafer-scale germanium substrate cleaning and reporosification advance membrane recycling, but repeated membrane production remains unverified.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.3390%2Fsu16041444

## Key claims

1. This process enables the fabrication of multiple high-quality monocrystalline Ge FSMs from the same substrate through efficient substrate reuse at a 100 mm wafer scale by a simple and low-cost chemical cleaning process.
   - Support: Tentative
   - Type: Primary finding
   - Basis: the demonstrated sequence ends at reporosification without growth and detachment of a second membrane
   - Location: Abstract
2. The new PGe layer presents a thickness of 265 ± 5 nm and a porosity of 63 ± 1%; both of these values are the same as on the original epi-ready substrate
   - Support: Supported
   - Type: Secondary
   - Basis: wafer-scale mapping supports similar layer properties for the demonstrated substrate without establishing between-wafer reproducibility
   - Location: Section 3, Figure 7
3. the developed process allows for both cost and an environmental impact reduction in Ge FSMs production, lowering the amount of Ge used per membrane fabrication.
   - Support: Tentative
   - Type: Secondary
   - Basis: estimated Ge savings lack comparative economic and environmental accounting
   - Location: Abstract
4. The lower porosity allows for more closely packed nucleation sites, resulting in a reduction in the membrane’s surface roughness to 0.7 nm from 1.2 nm on 70% porosity PGe substrate
   - Support: Tentative
   - Type: Secondary
   - Basis: the historical comparison changes porosity and layer thickness together without isolating the proposed roughness mechanism
   - Location: Section 3, paragraph after Figure 7
5. This results in over 100 membranes produced from a single 100 mm wafer.
   - Support: Tentative
   - Type: Secondary
   - Basis: the count extrapolates a thickness budget without repeated complete production cycles
   - Location: Section 3, material consumption paragraph

## Strengths

- **Recovered wafer retains mapped porous-layer uniformity** Ellipsometry mapping of the recovered 100 mm substrate gives a porous-layer thickness of 265 ± 5 nm and porosity of 63 ± 1%, close to the initial layer. This directly supports successful reporosification for the demonstrated wafer.
  - Dimension: contribution
  - Location: Section 3, Figures 3 and 7
- **Specified processing supports complementary material characterization** Methods report electrolyte composition, current waveform, growth conditions, and cleaning times. Ellipsometry, cross-sectional SEM, AFM, and in-plane XRD provide complementary measurements of layer structure, surface condition, and crystalline orientation.
  - Dimension: methodological rigour
  - Location: Sections 2.1–2.2; Figures 3–7
- **Alternative approaches receive explicit trade-off discussion** The discussion acknowledges the advantage of reconstructed porous structures above 400 °C and the potential substrate-reuse advantage of 2D-assisted epitaxy. It also identifies unresolved growth-area and interface-transfer challenges for the latter.
  - Dimension: positioning
  - Location: Section 3, final comparison paragraphs

## Limitations

- **Reuse stops before a second membrane** The reported sequence ends with a new porous layer on the recovered substrate, not a second grown and detached membrane. The abstract's multiple-membrane claim and the projected production counts therefore exceed the demonstrated sequence.
  - Dimension: reporting
  - Location: Abstract; Section 3, Figure 7 and material-consumption paragraph
- **Independent replication and yields remain unstated** The numbers of independent wafers, membranes, complete cycles, and AFM sampling locations are not specified. Without these counts or production-yield reporting, the spatial maps and representative images do not establish between-wafer reproducibility.
  - Dimension: methodological rigour
  - Location: Sections 2.1–2.2; Section 3, Figures 3–7
- **Economic and environmental claims exceed measurements** The paper estimates approximately 300 nm of substrate consumption per membrane but provides no comparative cost or environmental-impact assessment. Lower Ge consumption alone does not establish the overall benefits asserted in the abstract.
  - Dimension: reporting
  - Location: Abstract; Section 3, material-consumption discussion

## Reliability checks

Caveats (4 of 4 checks).

- **Results check:** Noted
  - "Indeed, while conventional Ge substrates have a thickness of 140 µm, 225 µm, and" (Section 1, paragraph 3 (substrate thickness)) vs "100 mm Ge wafer with a thickness of 175 µm, and its thinnest commercially available" (Section 3, paragraph on material consumption). The Introduction calls 140 µm conventional for 100 mm wafers, while Results assumes 175 µm conventional and 140 µm minimum, giving (175 − 140)/0.3 ≈ 117 projected membranes. The effect on the result is unclear.
- **Reporting and transparency:** Noted. The text includes an incorrect Figure 3 panel reference. Commercial conflicts are disclosed and data availability on request is stated; ethics review is not applicable.
  - Conflict of interest: declared · Data availability: declared
- **Reference integrity:** Clean. 55 of 55 checkable references verified
  - 60 references in manuscript
  - 5 have no canonical index record — counted, but not index-checkable
  - 2 references confirmed by manual review
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Clean
- **Summary:** No retraction or expression of concern found in Crossref (includes Retraction Watch).
- **Last checked:** 2026-11-25