# Low-Loss, Multi-Reticle-Stitched SiN Waveguides for 300 mm Wafer-Level Optical Interconnects

- **DOI:** [10.3390/photonics13010100](https://doi.org/10.3390/photonics13010100)
- **Rating:** Sound (3.5 out of 5)
- **Verdict:** A 300 mm stitched-SiN demonstration establishes low-loss wafer-scale routing, but measurement uncertainty limits precision of the smallest stitch-loss estimates.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.3390%2Fphotonics13010100

## Key claims

1. [300 mm wafer reticle-stitched LPCVD SiN waveguide technology] demonstrate a multi-reticle-stitched ~56 cm long waveguides across 20 reticles with propagation loss of 0.13~0.15 dB/cm at 1310 nm
   - Support: Supported
   - Type: Primary finding
   - Basis: spatially separated cutback measurements support low-loss routing but lack reported fit uncertainty and replication detail
   - Location: Abstract; Section 3; Fig. 2d
2. Because of the <5 nm lithography reticle offset, the stitch loss is calculated to be <0.001~0.002 dB
   - Support: Supported
   - Type: Secondary
   - Basis: matched-ring extraction supports a small upper bound, with unresolved matching precision at the smallest loss estimates
   - Location: Section 4
3. OVL measurements were fully conducted on four wafers (each wafer has 53 reticles, and each reticle has six OVL structures at separate locations on the mask scribe line), and the measured x- or y- reticle offset was <5 nm.
   - Support: Supported
   - Type: Secondary
   - Basis: extensive overlay readouts support the measured offsets, but scribe-line marks do not directly sample every waveguide stitch
   - Location: Section 4
4. [SiN waveguide] stitch loss increases to 0.002~0.005 dB due to the worse 20 nm y-offset.
   - Support: Tentative
   - Type: Secondary
   - Basis: one offset and one reference wafer per thickness leave wafer differences inseparable from the isolated offset effect
   - Location: Section 5

## Strengths

- **Long stitched routes on 300 mm wafers** Waveguides extend approximately 56 cm across 20 reticles, with reported propagation loss of 0.13~0.15 dB/cm at 1310 nm. This demonstrates a practical fabrication route for passive wafer-scale optical routing.
  - Dimension: contribution
  - Location: Section 3; Figure 2
- **Paired rings and deliberate offset validation** Reference and 12-stitch rings provide a differential loss measurement across eight wafers. A deliberate 20 nm offset and supporting simulations add a sensitivity check beyond baseline measurements.
  - Dimension: methodological rigour
  - Location: Sections 4–5; Figures 5–8; Appendix A.2
- **Explicit discussion of fabrication trade-offs** The paper acknowledges propagation loss above the cited <0.1 dB/cm state of the art and explains the integration-oriented fabrication choice. Table 1 also identifies the advanced lithography requirement.
  - Dimension: positioning
  - Location: Section 2, Table 1; Section 3

## Limitations

- **Cutback uncertainty and summary range remain unclear** The cutback measurements vary length and die location together without reporting fit uncertainty or replication detail. The Introduction and Conclusions give 0.12~0.15 dB/cm, versus 0.13~0.15 dB/cm in the Abstract and results.
  - Dimension: methodological rigour
  - Location: Abstract; Sections 1, 3 and 6; Figure 2d; Table A1
- **Small stitch signals challenge extraction precision** Table A1's stitch-loss spreads cross zero, and the confidence-interval construction does not establish how within-die pairing and wafer variation were handled. The imposed-offset comparison uses one offset and one reference wafer per thickness, limiting isolated causal attribution.
  - Dimension: methodological rigour
  - Location: Sections 4–5; Figures 6–8; Table A1; Appendix A.3
- **Prior stitch-loss benchmarking remains quantitatively incomplete** The platform comparison explains confinement and fabrication trade-offs but does not directly benchmark measured stitch loss against the closest cited demonstrations. This limits how precisely the advance over prior stitching can be judged.
  - Dimension: positioning
  - Location: Section 2, Table 1; Sections 3–4

## Reliability checks

Caveats (4 of 4 checks).

- **Results check:** Noted
  - "loss of 0.12~0.15 dB/cm at 1310 nm" (Section 1) vs "Waveguide loss: 0.131 ± 0.005 dB/cm" (Table A1, 300 nm thick SiN waveguide). Compare the 0.12 lower bound with the Abstract/results range and Table A1 central values, noting that the printed 300 nm lower endpoint is 0.131 − 0.005 = 0.126 dB/cm. The result itself is unaffected.
  - Minor reporting notes (1):
    - "Notably, the 2.5 µm wide taper-up stitch exhibits ~0.001 dB lower loss compared" (Section 5) vs "2.5 µm wide taper-up stitch can be 0.001~0.002 dB lower optical loss than the" (Figure 8 caption). Compare the text's approximate 0.001 dB taper-width benefit with the caption's 0.001~0.002 dB range, which shares that endpoint and preserves the direction. The result itself is unaffected.
- **Reporting and transparency:** Clean. Conflict-of-interest and data-availability declarations are present. Human and animal ethics review is appropriately declared not applicable to this physical fabrication study.
  - Conflict of interest: declared · Ethics approval: declared · Data availability: declared
- **Reference integrity:** Clean. 18 of 18 checkable references verified
  - 18 references in manuscript
  - 1 reference confirmed by manual review
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Clean
- **Summary:** No retraction or expression of concern found in Crossref (includes Retraction Watch).
- **Last checked:** 2026-11-25