# Ultraviolet to mid-infrared optical properties of sputtered Al(Sc)N-on-SiO 2 thin films and experimental demonstration of AlN integrated photonic devices in the telecom C-band

- **DOI:** [10.1364/oe.540975](https://doi.org/10.1364/oe.540975)
- **Rating:** Sound (3.5 out of 5)
- **Verdict:** Broadband AlScN optical characterization extends design data into the mid-infrared, but the device demonstration remains confined to undoped AlN.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.1364%2Foe.540975

## Key claims

1. At a wavelength of 1.55 µm, commonly used for fiber-optical telecommunications, an increase of the real part of refractive index is observed with higher Sc doping
   - Support: Supported
   - Type: Primary finding
   - Basis: consistent fitted-index trends across measured films with unreported uncertainty and a different deposition bias for the undoped baseline
   - Location: Section 2.2
2. Our fabricated AlN waveguides exhibit a propagation loss of 6.2 dB/cm, and an ORR demonstrates a loaded Q-factor of 33,965.
   - Support: Supported
   - Type: Secondary
   - Basis: complementary loss measurements support the reported devices despite unspecified replication and uncertainty
   - Location: Introduction; Sections 3.1, 3.2
3. the imaginary part (extinction coefficient) of the refractive index also increases slightly, indicating increased material losses at higher Sc concentrations
   - Support: Tentative
   - Type: Secondary
   - Basis: unvalidated near-infrared ellipsometric sensitivity limits interpretation of fitted extinction coefficients as material absorption
   - Location: Section 2.2
4. a significant improvement in sidewall roughness [of etched AlN structures] can be observed following the introduction of the [Ar] plasma treatment step, with the effect saturating after 2.5 minutes
   - Support: Tentative
   - Type: Secondary
   - Basis: qualitative SEM images without quantitative sidewall metrology or optical-loss comparisons
   - Location: Section 3, p. 7, Fig. 4
5. The anisotropic bandgap values retrieved via spectroscopic ellipsometry in both ordinary and extraordinary directions decreases with increasing Sc concentration
   - Support: Supported
   - Type: Secondary
   - Basis: consistent decreases in both fitted bandgap series despite unreported fit uncertainty and film-to-film variation
   - Location: Section 2.2

## Strengths

- **Broadband optical characterization on relevant substrates** Anisotropic optical characterization spans 0.19–25 µm for four Sc compositions on SiO2, extending the reported data into the mid-infrared phonon region.
  - Dimension: contribution
  - Location: Section 2.2, Fig. 2 and Table 1
- **Complementary measurements support device loss estimates** The 6.2 dB/cm cut-back result agrees with the 6.19 dB/cm ring-derived estimate under the stated under-coupling assumption. The reported resonance width also reproduces the loaded Q-factor of 33,965.
  - Dimension: methodological rigour
  - Location: Sections 3.1–3.2, Fig. 6
- **Device performance benchmarked against close precedents** The discussion directly compares its measured Q-factor with earlier AlN devices and acknowledges its position at the lower end of comparable results.
  - Dimension: positioning
  - Location: Introduction; Section 3.2

## Limitations

- **Replication and uncertainty reporting limit precision** Independent wafer, die and device replication counts and uncertainty estimates are not reported for the principal optical constants and device figures. The undoped film also uses a different substrate bias from the doped films, limiting attribution to Sc alone.
  - Dimension: methodological rigour
  - Location: Sections 2.1–2.2, Table 1; Sections 3.1–3.2
- **Fitted extinction coefficients lack loss validation** The near-infrared fitted extinction coefficients are interpreted as material-loss indicators without independent validation at that sensitivity. Their relationship to the measured low device loss remains unresolved because the film and waveguide measurements are not directly equivalent.
  - Dimension: methodological rigour
  - Location: Section 2.2, Table 1; Sections 3.1–3.2
- **Fabrication evidence stops at undoped AlN** All fabricated components use undoped AlN, leaving adaptation to Sc-doped films untested. Sidewall smoothing is assessed through SEM images rather than quantitative roughness or before-and-after optical loss.
  - Dimension: contribution
  - Location: Section 3, Fig. 4; Section 4

## Reliability checks

Caveats (3 of 4 checks).

- **Results check:** Noted. One reported value does not reconcile, but the key claims do not rest on it.
  - Minor reporting notes (1):
    - "As the Sc concentration increases, there is a corresponding rise in surface roughness" (Section 2.1, surface morphology) vs "yielding 0.33 nm, 7.51 nm, 11.35 nm and 9.37 nm for the 0%, 5.8%, 16.9%, and 37.8% Sc samples, respectively." (Section 2.1, surface morphology). The listed RMS roughness decreases from 11.35 nm at 16.9% Sc to 9.37 nm at 37.8% Sc, while every doped value exceeds the undoped value. The result itself is unaffected.
- **Reporting and transparency:** Clean. Funding and conflict-of-interest disclosures are present, and underlying data are offered on reasonable request. No supplied-text research-conduct concern is established.
  - Conflict of interest: declared · Data availability: declared
- **Reference integrity:** Clean. 52 of 52 checkable references verified
  - 54 references in manuscript
  - 2 have no canonical index record — counted, but not index-checkable
  - 7 references confirmed by manual review
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Not checked
- **Summary:** Post-publication record check unavailable at this time.
- **Last checked:** 2026-11-25