# Optical Degradation of 845 nm VCSELs With Different Oxide Apertures for Silicon Photonics

- **DOI:** [10.1109/jstqe.2026.3702031](https://doi.org/10.1109/jstqe.2026.3702031)
- **Rating:** Limited (2.8 out of 5)
- **Verdict:** Accelerated VCSEL tests support a thermal explanation for aperture-dependent degradation, but the abstract reverses the measured aperture–onset-current relationship.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.1109%2Fjstqe.2026.3702031

## Key claims

1. The experimental results showed that devices with a larger oxide aperture exhibit better reliability.
   - Support: Tentative
   - Type: Primary finding
   - Basis: accelerated comparisons with unstated device counts do not establish reliability across operating conditions
   - Location: Abstract
2. From the analysis of the degradation kinetics, we found that the current at which the highly accelerated degradation process occurs depends inversely on the aperture radius.
   - Support: Unsupported
   - Type: Secondary
   - Basis: reported onset currents increase with aperture radius and support approximately direct, not inverse, proportionality
   - Location: Abstract; Section IV.A, Figure 2b
3. devices with a larger aperture have lower thermal impedance, and therefore operate at lower internal temperatures at similar bias points
   - Support: Supported
   - Type: Secondary
   - Basis: measured thermal-impedance trends support the direction despite temperature-calibration extrapolation
   - Location: Abstract; Section IV.B, Fig. 3a
4. when the same internal temperature is maintained during ageing, for all VCSEL geometries under study the onset of degradation occurs at the same time
   - Support: Tentative
   - Type: Secondary
   - Basis: unequal extrapolated temperature estimates and unstated replication limit the claimed isothermal equivalence
   - Location: Abstract; Section IV.C, Fig. 4
5. The equivalent activation energy of the degradation process was found to fall between 0.43 and 0.68 eV.
   - Support: Tentative
   - Type: Secondary
   - Basis: three-temperature extraction with unstated device counts and extrapolated junction temperatures leaves the range poorly characterized
   - Location: Abstract; Section IV.D, Fig. 5b

## Strengths

- **Complementary measurements connect geometry and heating** Radius-normalized step-stress curves, pulsed thermal-impedance measurements and constant-current ageing provide complementary evidence for a thermal explanation of aperture-dependent degradation.
  - Dimension: methodological rigour
  - Location: Sections IV.A–C; Figures 2–4
- **Temperature series extends the degradation comparison** Ageing at three baseplate temperatures adds evidence that higher internal temperature accelerates rapid degradation and yields a reported equivalent activation-energy range of 0.43–0.68 eV.
  - Dimension: contribution
  - Location: Section IV.D; Figure 5
- **Operating limits and design tradeoffs acknowledged** The text identifies temperature-extrapolation uncertainty and stresses beyond practical operation. The conclusion also explains the trade-off between lower thermal impedance and optical performance as aperture size increases.
  - Dimension: positioning
  - Location: Sections IV.C–D; Conclusions

## Limitations

- **Abstract reverses the measured scaling relationship** The abstract states an inverse dependence on aperture radius, but onset currents rise from approximately 4 to 6.5 mA as aperture diameter increases from 4 to 6 µm. The measurements support approximately direct proportionality instead.
  - Dimension: methodological rigour
  - Location: Abstract; Section IV.A; Figure 2
- **Independent device counts are not reported** The number of devices tested per aperture and temperature is unstated, and device-to-device variability is not quantified. This limits confidence in both the reliability comparison and the activation-energy range.
  - Dimension: methodological rigour
  - Location: Section III; Section IV.D; Figures 2–5
- **Isothermal wording exceeds demonstrated temperature matching** The abstract describes the same maintained internal temperature, while Figure 4 gives estimated temperatures of 134, 127 and 126 °C. Those estimates extrapolate beyond the 20–70 °C calibration range, making the comparison suggestive rather than an exact isothermal demonstration.
  - Dimension: reporting
  - Location: Abstract; Sections IV.B–C; Figure 4

## Reliability checks

Caveats (4 of 4 checks).

- **Results check:** Noted
  - "the current at which the highly accelerated degradation process occurs depends inversely on the aperture radius" (Abstract) vs "≈6.5 mA) compared to the other two devices (≈5.5 mA for the 5 µm aperture and ≈4 mA for the 4 µm aperture device" (Section IV.A). Dividing the reported onset currents of approximately 4, 5.5 and 6.5 mA by radii of 2, 2.5 and 3 µm gives approximately 2.0, 2.2 and 2.17 mA/µm, demonstrating approximately direct rather than inverse proportionality. The claim is not supported by the paper's own data.
  - "5 µm aperture device, from which a thermal impedance of about" (Section IV.B (text describing Fig. 3b)) vs "(4 µm oxide aperture VCSEL)" (Figure 3 caption). The results text assigns Figure 3b to a 5 µm aperture device, whereas its caption assigns it to a 4 µm aperture device; the separate trend in Figure 3a is unaffected. The result itself is unaffected.
  - "three different TTF conditions: +25 %, +50%, and +70% degradation of the Ith." (Fig. 5 caption) vs "increase the initial threshold current of the device by specific amounts: 25%, 50%, and 75%." (Section IV.D, paragraph 2). The third threshold-current failure criterion is +70% in the caption but +75% in the results text and panel legend, preventing an unambiguous identification of the criterion underlying the reported range. The effect on the result is unclear.
- **Reporting and transparency:** Clean. No research-conduct concern is established by the supplied text. Missing availability and disclosure statements are treated as unknown, and the caption conflicts are recorded under Internal Coherence.
- **Reference integrity:** Clean
  - 23 references in manuscript
  - 23 of 23 checkable references found in an index
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Clean
- **Summary:** No retraction or expression of concern found in Crossref (includes Retraction Watch).
- **Last checked:** 2026-11-25