# Impact of the Oxide Aperture Width on the Degradation of 845 Nm VCSELs for Silicon Photonics

- **DOI:** [10.1109/jstqe.2024.3415674](https://doi.org/10.1109/jstqe.2024.3415674)
- **Rating:** Sound (3.0 out of 5)
- **Verdict:** Aperture comparisons and beam-profile measurements extend evidence on 845 nm VCSEL degradation, but single-device sampling prevents a general reliability design rule.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.1109%2Fjstqe.2024.3415674

## Key claims

1. Thanks to our analysis we proved that the use of a larger aperture can result in a better device reliability.
   - Support: Tentative
   - Type: Primary finding
   - Basis: one device per aperture and resistance drift rather than lifetime testing cannot establish a general reliability improvement
   - Location: Abstract; Section VI
2. The results of this set of experiments showed that the electrical degradation is stronger as the oxide aperture is smaller, and mostly depends on the contribution of the top DBR resistance.
   - Support: Tentative
   - Type: Secondary
   - Basis: single-device aperture comparisons and assumed unchanged aperture resistance do not independently identify the top DBR contribution
   - Location: Abstract; Section V-A, Fig. 7, Fig. 8
3. Based on numerical simulations, we demonstrated that the electrical degradation (increase in series resistance) is responsible for a larger current spreading which, in turn, increases the FWHM (full width half maximum) of the optical beam.
   - Support: Tentative
   - Type: Secondary
   - Basis: simulations impose impurity profiles and establish compatibility rather than uniquely identifying the cause of measured beam broadening
   - Location: Abstract; Section IV-C, Fig. 6
4. The experimental results showed an increased spreading of the optical beam of the VCSEL with increasing ageing time.
   - Support: Supported
   - Type: Secondary
   - Basis: direct below-threshold emission profiles document broadening in one device, with low late-stage signal-to-noise limiting precision
   - Location: Abstract; Section IV-A, Fig. 2
5. the findings of our study can be considered valid for any AlGaAs-based bottom-emitting VCSELs operating at 850 nm.
   - Support: Tentative
   - Type: Secondary
   - Basis: one epitaxial design and unreplicated aperture conditions do not establish validity across all such devices
   - Location: Section VI, Conclusion

## Strengths

- **Beam profiles extend device degradation measurements** Spatial electroluminescence tracking adds beam-width evolution to the electrical degradation measurements, allowing their two-phase kinetics to be compared directly.
  - Dimension: contribution
  - Location: Section IV-A, Figs. 2–3
- **Microscopy tests an alternative defect explanation** Aged and unaged structures are examined for extended defects near the oxide aperture. The discussion explicitly distinguishes the absence of observed extended defects from the inability to detect isolated point defects or low-concentration impurities.
  - Dimension: methodological rigour
  - Location: Section IV-B, Fig. 5
- **Practical aperture design tradeoff is explicit** The conclusion connects aperture choice to competing requirements for resistance stability, low threshold current, and single-mode operation.
  - Dimension: positioning
  - Location: Section VI

## Limitations

- **Single-device comparisons cannot establish population reliability** The optical test uses one 7 μm device, and the aperture comparison uses one device at each of four sizes. Device-to-device variability and statistical lifetime reliability therefore remain unmeasured.
  - Dimension: methodological rigour
  - Location: Section III; Section V-A, Figs. 7–8
- **Resistance model misses the initial geometry contrast** The initial resistance ratio is 393/77 ≈ 5.10, above the maximum aperture-only model ratio of (7/4)² ≈ 3.06. Attribution of degradation primarily to the top DBR also depends on holding aperture resistance unchanged rather than independently distinguishing its contribution.
  - Dimension: methodological rigour
  - Location: Sections V-A–B; Appendix A
- **Definitive language exceeds the demonstrated evidence** The Abstract describes reliability improvement as proved and the mechanism as demonstrated, although the evidence comprises unreplicated device comparisons and simulations with assumed impurity profiles. The conclusion also extends validity to any AlGaAs-based bottom-emitting 850 nm VCSEL.
  - Dimension: reporting
  - Location: Abstract; Sections I, IV-C, and VI

## Reliability checks

Caveats (4 of 4 checks).

- **Results check:** Noted. 2 reported values do not reconcile, but the key claims do not rest on them.
  - Minor reporting notes (2):
    - "below threshold at 200 μA (≈260 A/cm2)" (Section IV-A, Experimental Analysis) vs "constant current stress at 10 mA (≈26 kA/cm2)" (Section VI, Conclusion). 10 mA/200 μA = 50, so 26 kA/cm2 divided by 50 is 520 A/cm2 rather than 260 A/cm2 for the same device. The result itself is unaffected.
    - "transferred onto a glass substrate" (Section II, paragraph 2) vs "The chip was placed onto a sapphire window" (Section III, paragraph 1). The transfer description names glass while the measurement description names a sapphire window, without explicitly explaining their relationship. The result itself is unaffected.
- **Reporting and transparency:** Clean. No substantiated research-conduct or transparency anomaly is established in the supplied text. Missing availability statements and ordinary typographical errors do not establish such an anomaly.
  - Conflict of interest: not stated · Data availability: not stated · Code availability: not stated
- **Reference integrity:** Clean
  - 14 references in manuscript
  - 14 of 14 checkable references found in an index
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Clean
- **Summary:** No retraction or expression of concern found in Crossref (includes Retraction Watch).
- **Last checked:** 2026-11-25