# Ultra-Low Loss and Large Bandwidth Fiber-to-Chip Edge Coupler for Aluminum Oxide Photonic Platform at UV-Visible Wavelengths

- **DOI:** [10.1109/jlt.2025.3567712](https://doi.org/10.1109/jlt.2025.3567712)
- **Rating:** Sound (3.2 out of 5)
- **Verdict:** A SiOx/AlOx edge coupler advances near-UV and blue fiber coupling, but subtraction-dominated measurements leave its headline sub-decibel precision unestablished.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.1109%2Fjlt.2025.3567712

## Key claims

1. The coupling loss between a standard single-mode fiber and an AlOx waveguide below 0.31 dB and 0.62 dB is experimentally demonstrated at a working wavelength of 375 nm and 405 nm, respectively.
   - Support: Tentative
   - Type: Primary finding
   - Basis: subtraction-dominated two-device measurements leave the precise loss thresholds sensitive to unquantified systematic error
   - Location: Abstract; Sec. IV
2. The design exhibits a large bandwidth of 110 nm below 2.6-dB loss over the entire operating wavelength range of the single mode fiber, as obtained from the simulation.
   - Support: Supported
   - Type: Secondary
   - Basis: reported simulations support the explicitly theoretical bandwidth, with experimental validation limited to two wavelengths
   - Location: Abstract; Sec. IV, Fig. 6(e)
3. We have proposed an ultra-low-loss edge coupler that operates effectively across the UVC and visible spectrum, demonstrating its viability at wavelengths of 375 nm and 405 nm.
   - Support: Tentative
   - Type: Secondary
   - Basis: the UVC clause conflicts with the reported wavelength range despite measurements supporting viability at 375 and 405 nm
   - Location: Section V, paragraph 1
4. This coupler not only facilitates low-loss fiber-to-chip coupling but also significantly reduces spurious light scattering
   - Support: Tentative
   - Type: Secondary
   - Basis: qualitative scattering images without a reference comparison cannot establish a significant reduction
   - Location: Abstract; Conclusion

## Strengths

- **Mode conversion addresses a documented coupling gap** The SiOx/AlOx architecture targets the mode mismatch between commercial single-mode fibers and small AlOx waveguides. The introduction establishes a concrete comparison with cited edge-coupler losses of approximately 3–6.7 dB.
  - Dimension: contribution
  - Location: Sections I–II
- **Simulation sweeps test practical design sensitivities** Mode-overlap and eigenmode-expansion calculations examine waveguide dimensions, taper length, fiber displacement, and taper-tip width. These analyses support the design choices while keeping tolerance evidence distinct from experimental validation.
  - Dimension: methodological rigour
  - Location: Section II, Figs. 2–3
- **Microscopy documents the fabricated device geometry** SEM images characterize the etched SiOx cross-section and report an AlOx taper-tip width of 61.6 ± 4.6 nm. This provides physical checks on the fabricated structures used for optical testing.
  - Dimension: methodological rigour
  - Location: Section III, Fig. 5

## Limitations

- **Loss extraction lacks an independent transmission control** The headline estimate subtracts about 6.97 dB of camera-derived propagation loss from about 7.59 dB of total insertion loss. Without a cut-back or equivalent independent reference, calibration offsets can materially alter the small residual.
  - Dimension: methodological rigour
  - Location: Section IV, Fig. 6
- **Through transmission identifies only the facet average** The two-interface measurement yields a combined coupling loss, whose halving estimates the mean rather than either facet individually. The printed equation omits that division, although adding it reproduces the rounded 0.31 dB/facet result.
  - Dimension: methodological rigour
  - Location: Section IV, coupling-loss calculation
- **UVC and scattering statements exceed reported evidence** The conclusion claims UVC operation despite a reported 320–430 nm low-loss range and measurements at 375 and 405 nm, outside UVC. The abstract also asserts significant scattering reduction without a quantified reference comparison.
  - Dimension: reporting
  - Location: Abstract; Section IV, Fig. 6; Section V

## Reliability checks

Caveats (4 of 4 checks).

- **Results check:** Noted
  - "The coupling loss is calculated as: αEC = −10*log(Pfpf/Pin)-α PIC." (Section IV, coupling-loss equation) vs "the coupling loss is estimated to be 0.31 dB/facet." (Section IV, 375-nm TE measurement). The stated powers and propagation loss give −10 log10(0.61/3.5) − 12.02 × 0.58 ≈ 0.615 dB total, which becomes approximately 0.308 dB per facet after division by two. The result itself is unaffected.
  - "In conclusion, We have proposed an ultra-low-loss edge coupler that operates effectively across the UVC and visible spectrum, demonstrating its viability at wavelengths of 375 nm and 405 nm." (Section V, paragraph 1) vs "achieving coupling losses of less than 2.6 dB per facet from 320 to 350 nm" (Section IV, paragraph 2). The reported 320–430 nm low-loss range and 375/405 nm measurements are outside UVC, defined as 100–280 nm, contradicting the UVC clause but not the measured-wavelength clause. The claim is not supported by the paper's own data.
- **Reporting and transparency:** Noted. The fabrication description starts from bare silicon without explaining the thermal oxide undercladding assumed in the optical design. This is a methods-reporting omission, not evidence of improper conduct.
- **Reference integrity:** Clean. 25 of 25 checkable references verified
  - 25 references in manuscript
  - 5 references confirmed by manual review
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Clean
- **Summary:** No retraction or expression of concern found in Crossref (includes Retraction Watch).
- **Last checked:** 2026-11-25