# Ultra-high endurance silicon photonic memory using vanadium dioxide

- **DOI:** [10.1038/s44310-024-00038-1](https://doi.org/10.1038/s44310-024-00038-1)
- **Rating:** Sound (3.2 out of 5)
- **Verdict:** VO2 photonic memory extends demonstrated cycling endurance, but separate endurance and transient-switching experiments leave its combined performance unproven.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.1038%2Fs44310-024-00038-1

## Key claims

1. Here, we report an ultra-high endurance silicon photonic volatile memory using vanadium dioxide (VO2) exhibiting a record cyclability of up to 10^7 cycles without degradation.
   - Support: Tentative
   - Type: Primary finding
   - Basis: single-device endurance evidence relies on intermittent sampling and recovered contrast after realignment
   - Location: Abstract; Results, Endurance measurements, Fig. 2(a)–(c)
2. Hence, an energy pulse of 24 pJ was sufficient to switch back and forth the VO2 patch [of 1 µm length] with switching times as fast as 24 and 36 ns, respectively.
   - Support: Tentative
   - Type: Secondary
   - Basis: single-pulse transient switching on a separate device does not establish latched memory write and erase
   - Location: Results, Speed and energy consumption performance, Fig. 3
3. [Compared to Ge2Sb2Te5 (GST)], our experimental results lead to a switching energy density of 0.4 aJ nm−3 to write the state, which is one order of magnitude lower than experimental state-of-the-art GST photonic memories (8 aJ nm−3)
   - Support: Tentative
   - Type: Secondary
   - Basis: pulse-energy benchmarking excludes continuous holding energy and leaves the optical calibration basis unspecified
   - Location: Results, Speed and energy consumption performance, Fig. 4
4. Moreover, the distribution of the optical transmission readout, shown in Fig. 2(d), revealed a remarkable accuracy of ±0.11 dB in the erased state and ±0.085 dB in the written state for the standard deviation.
   - Support: Supported
   - Type: Secondary
   - Basis: one-device readout distributions at 4×10^6 cycles support repeatability estimates despite an unstated histogram sample count
   - Location: Results, Endurance measurements, Fig. 2(d)

## Strengths

- **Cycling demonstration extends photonic memory endurance** The VO2/Si device demonstrates operation through 10^6 cycles before alignment-related contrast loss, with recovered contrast reported after cycling beyond 10^7. This extends the endurance range discussed for chalcogenide photonic memories.
  - Dimension: contribution
  - Location: Introduction; Results, Endurance measurements; Fig. 2(a)–(c)
- **Distinct optical signals separate programming and readout** The counter-propagating setup uses a 1550 nm programming signal and a separate 1565 nm readout probe. Methods also describes fabrication and real-time chip-transmission monitoring.
  - Dimension: methodological rigour
  - Location: Methods, Experimental set-up and Fabrication process
- **Readout distributions quantify binary state separation** The endurance device provides approximately 2.6 dB contrast, with reported readout standard deviations of ±0.11 dB and ±0.085 dB. These measurements quantify repeatability at the sampled cycling point.
  - Dimension: methodological rigour
  - Location: Results, Endurance measurements; Fig. 2(d)

## Limitations

- **Drift complicates the unqualified endurance headline** Only five cycles are recorded per 10,000, and declining contrast above 10^6 cycles is recovered by realignment without shown reference-normalized drift data. This supports a narrower interpretation than uninterrupted operation 'without degradation' on the single tested device.
  - Dimension: methodological rigour
  - Location: Abstract; Results, Endurance measurements; Fig. 2(a)–(c); Methods
- **Fast switching remains separate from endurance** The endurance result uses a 3 µm device with 1 µs pulses, whereas the 24 pJ result uses single approximately 100 ns pulses on a 1 µm device. The latter measures transient switching rather than demonstrating equally fast latched memory cycling with the reported endurance.
  - Dimension: methodological rigour
  - Location: Results, Endurance measurements and Speed and energy consumption performance; Figs. 2–3
- **Holding power limits broader energy comparisons** The disclosed 180 µW holding power corresponds to 18 nJ over a 100 µs endurance-test period. Figure 4 compares programming energy, but the broader low-energy application discussion does not account for continuous holding energy and does not establish total operating energy for the separate 1 µm device.
  - Dimension: positioning
  - Location: Results, Endurance measurements and Fig. 4 comparison; Discussion

## Reliability checks

Caveats (3 of 4 checks).

- **Results check:** Noted. One reported value does not reconcile, but the key claims do not rest on it.
  - Minor reporting notes (1):
    - "235 𝐽𝐽 𝑐𝑐𝑚𝑚−3, the specific heat capacity20, 𝐶𝐶= 3 𝐽𝐽 𝑐𝑐𝑚𝑚−3𝐾𝐾−1" (Results, Speed and energy consumption performance) vs "energy density of 𝐻𝐻+ 𝐶𝐶 Δ𝑇𝑇= 0.31 𝑎𝑎𝑎𝑎 𝑛𝑛𝑚𝑚−3 , where Δ𝑇𝑇= 65 −25 oC" (Results, Speed and energy consumption performance). The stated formula gives 235 + 3 × (65 − 25) = 355 J cm−3 = 0.355 aJ nm−3 rather than 0.31 aJ nm−3, without overturning the measured switching results. The result itself is unaffected.
- **Reporting and transparency:** Clean. Competing interests and data availability upon reasonable request are declared. No supplied-text reporting or transparency concern is established, and human or animal ethics approval is not applicable.
  - Conflict of interest: declared · Data availability: declared
- **Reference integrity:** Clean. 32 of 32 checkable references verified
  - 32 references in manuscript
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Not checked
- **Summary:** Post-publication record check unavailable at this time.
- **Last checked:** 2026-11-25