# Lithium tantalate photonic integrated circuits for volume manufacturing.

- **DOI:** [10.1038/s41586-024-07369-1](https://doi.org/10.1038/s41586-024-07369-1)
- **Rating:** Strong (4.0 out of 5)
- **Verdict:** Lithium tantalate circuits combine low loss, electro-optic modulation and soliton generation at wafer scale, but production economics remain unmeasured.
- **Framework version:** v5.13
- **Pipeline version:** v0.4
- **Evaluation date:** 2026-11-25
- **Evaluation page:** https://www.nabu.science/paper/10.1038%2Fs41586-024-07369-1

## Key claims

1. We show that LiTaO3 can be etched to create low-loss (5.6 dB m-1) PICs using a deep ultraviolet (DUV) stepper-based manufacturing process
   - Support: Supported
   - Type: Primary finding
   - Basis: selected-resonance performance supported by wafer mapping and spiral measurements, without production-yield or cost validation
   - Location: Abstract
2. We demonstrate a LiTaO3 Mach-Zehnder modulator (MZM) with a half-wave voltage-length product of 1.9 V cm and an electro-optic bandwidth of up to 40 GHz.
   - Support: Supported
   - Type: Secondary
   - Basis: direct device measurements with limited replication and unspecified receiver-response de-embedding
   - Location: Abstract
3. In comparison with LiNbO3, LiTaO3 exhibits a much lower birefringence, enabling high-density circuits and broadband operation over all telecommunication bands.
   - Support: Tentative
   - Type: Secondary
   - Basis: one device-pair dispersion comparison and simulations do not demonstrate high-density circuits
   - Location: Abstract; Results, LiTaO3 PICs; Fig. 2e-i
4. In each of the ten tested devices with the orientation θ = 90°, solitons were consistently generated. Conversely, none of the attempts to generate solitons were successful in the ten devices oriented at θ = 0°.
   - Support: Supported
   - Type: Secondary
   - Basis: replicated orientation contrast bounded to the tested devices rather than an isolated Raman mechanism
   - Location: Results, Soliton-microcomb generation; Fig. 4
5. Our platform is capable of processing signals across all optical communications bands (1,260–1,620 nm) in a single PIC, owing to the successful suppression of fundamental mode mixing.
   - Support: Tentative
   - Type: Secondary
   - Basis: broadband dispersion and two-wavelength modulation do not establish signal processing across every communications band
   - Location: Summary

## Strengths

- **Loss measurements cross-checked by independent methods** Wafer-scale resonator mapping is complemented by 39 cm spiral-waveguide reflectometry and thermal-response separation of absorption from scattering. These measurements support the low-loss platform beyond a selected resonance.
  - Dimension: methodological rigour
  - Location: Fig. 2a–d; Extended Data Fig. 2
- **One platform demonstrates modulation and solitons** The circuits demonstrate a 1.9 V cm modulator voltage-length product and soliton generation at 81 GHz and 30.1 GHz repetition rates. Solitons were reported in all ten devices at one orientation and none of ten at the other.
  - Dimension: contribution
  - Location: Figs. 3–4; Soliton-microcomb generation
- **Competing platforms receive explicit performance comparisons** Lithium-niobate comparisons address birefringence, dispersion and photorefraction. The soliton discussion also acknowledges higher measured phase noise than earlier silicon-nitride and z-cut lithium-niobate systems.
  - Dimension: positioning
  - Location: Fig. 2e–i; Extended Data Fig. 3; Soliton-microcomb generation

## Limitations

- **Central framing exceeds demonstrated operating scope** Low-cost volume production is not established by cost or yield measurements, and the headline 5.6 dB/m loss is a selected resonance rather than a wafer average. The all-band signal-processing conclusion also extends beyond broadband dispersion measurements and modulation at two wavelengths.
  - Dimension: reporting
  - Location: Title; Abstract; Fig. 2; Fig. 3; Summary
- **Device comparisons lack replication and uncertainty** The modulator and material comparisons rely on individual devices or samples without repeat-device uncertainty estimates. Raman suppression is inferred from free-space film measurements rather than directly measured cavity Raman gain.
  - Dimension: methodological rigour
  - Location: Electro-optical modulation; Methods, Photorefractive effect comparison; Methods, Soliton and Raman measurement
- **Raman polarization directions conflict across sections** The main text says Raman intensity decreases from y-polarized to z-polarized excitation, whereas Methods states the reverse. This leaves the mechanistic explanation unclear without disproving the reported soliton counts.
  - Dimension: reporting
  - Location: Soliton-microcomb generation; Methods, Soliton and Raman measurement

## Reliability checks

Caveats (4 of 4 checks).

- **Results check:** Noted
  - "A reduction in Raman intensity was achieved when the polarization of incident light transitions from being parallel to the y axis to being parallel to the z axis" (Results, Soliton-microcomb generation, Raman paragraph) vs "The Raman intensity becomes lower when the polarization of incident light transitions from being parallel to the z axis to being parallel to the y axis." (Methods, Soliton and Raman measurement). The passages state opposite polarization directions for decreasing Raman intensity, leaving the mechanistic description unresolved but not contradicting the reported device counts. The effect on the result is unclear.
  - "at a wavelength of 1.55 μm lies at around 700 nm" (Results, LiTaO3 PICs, birefringence paragraph (critical thickness)) vs "For LiNbO3, we found a crossing of the fundamental TE and TM modes at an angle of 25°" (Results, LiTaO3 PICs, birefringence paragraph (simulation)). The reported crossing in the simulation described as using a 600 nm waveguide appears below the approximately 700 nm threshold, although equivalence of the thickness definitions is uncertain. The effect on the result is unclear.
  - "The etching depth was 220 nm, leaving a 400 nm slab." (Results, Electro-optical modulation, MZM paragraph) vs "thin the LiTaO3 film to the desired thickness of 600 nm" (Methods, LTOI wafer fabrication). The stated etch and slab sum to 620 nm rather than the nominal 600 nm, with the 20 nm difference potentially accommodated by the reported wafer non-uniformity. The result itself is unaffected.
  - Minor reporting notes (1):
    - "The 30.1 GHz single-soliton state features a bandwidth of 4.0 THz and supports a pulse duration of 71 fs." (Results, Soliton-microcomb generation) vs "spectral bandwidth of the 81 GHz single soliton is 4.9 THz, corresponding to a pulse duration of 63 fs" (Results, Soliton-microcomb generation). Assuming a sech² time-bandwidth product of 0.315 gives approximately 79 fs for 4.0 THz and 64 fs for 4.9 THz, with fitted rather than stated bandwidth potentially explaining the first difference. The result itself is unaffected.
- **Reporting and transparency:** Clean. Data and plotting code availability are declared at a persistent Zenodo identifier, and competing interests are disclosed. No conduct finding is retained.
  - Conflict of interest: declared · Data availability: declared · Code availability: declared
- **Reference integrity:** Clean. 1 of 1 checkable references verified
  - 1 reference in manuscript
  - References not verified automatically are resolved manually within 24 hours.

## Post-publication record

- **Status:** Clean
- **Summary:** No retraction or expression of concern found in Crossref (includes Retraction Watch).
- **Last checked:** 2026-11-25